Effective Utilization of Fly Ash, Iron Ore Slime and LD-Slag in Geopolymer Mortar

著者

  • Rajesh Chintala
  • R. K. Rath
  • Anil Kumar

キーワード:

Fly Ash、 LD-Slag、 Geopolymer、 Compressive Strength、 NaOH、 Iron ore Slime

要旨

AbstractAn attempt was made for the effective utilization of iron ore slime in making of geopolymer mortar along with other industrial wastes fly ash and LD-slag and achieved the appreciable compressive strength results with 8 M NaOH after 28 days at a curing period of 24 h at 55°C.  Keywords: Fly ash, LD-slag, geopolymer, compressive strength, NaOH, iron ore slimeCite this Article  Rajesh Chintala, R.K. Rath, Anil Kumar. Effective Utilization of Fly Ash, Iron Ore Slime and LD-Slag in Geopolymer Mortar. Recent Trends in Civil Engineering & Technology. 2017; 7(1): 9–16p.